    Superstrength through nanotwinning 

    An, Qi; Goddard III, William A.; Xie, Kelvin Y.; Sim, Gi-dong; Hemker, Kevin J.; Munhollon, Tyler; Toksoy, M. Fatih; Haber, Richard A. (American Chemical Society, 2016)
    The theoretical strength of a material is the minimum stress to deform or fracture the perfect single crystal material that has no defects. This theoretical strength is considered as an upper bound on the attainable strength ...